详细信息

Multi-environment responsiveness triblock copolymer used for optical information storage, comprises polyethylene glycol-b-polymethylacrylic acid dimethylamine ethyl ester-b-polyazobenzene tri-block copolymer    

文献类型:专利

英文题名:Multi-environment responsiveness triblock copolymer used for optical information storage, comprises polyethylene glycol-b-polymethylacrylic acid dimethylamine ethyl ester-b-polyazobenzene tri-block copolymer

作者:ZHUANG Z;XING Y;LIN S;HE X;LIN J;ZHUANG Q;ZHU W

机构:[1]UNIV EAST CHINA SCI&TECHNOLOGY

申请号:CN102633960-A

申请日:2012-04-01

公开日:2012-08-15

语种:英文

收录:DERWENT

摘要:NOVELTY - A multi-environment responsiveness triblock copolymer comprises polyethylene glycol-b-polymethylacrylic acid dimethylamine ethyl ester-b-polyazobenzene tri-block copolymer which is obtained by polyethylene glycol-b-polymethylacrylic acid dimethylamine ethyl ester di-block copolymer triggering azo phenyl monomer. USE - A multi-environment responsiveness triblock copolymer for optical information storage (claimed). ADVANTAGE - The multi-environment responsiveness triblock copolymer has desired response to light, temperature and pH value. DETAILED DESCRIPTION - A multi-environment responsiveness triblock copolymer comprises polyethylene glycol-b-polymethylacrylic acid dimethylamine ethyl ester-b-polyazobenzene tri-block copolymer which is obtained by polyethylene glycol-b-polymethylacrylic acid dimethylamine ethyl ester di-block copolymer triggering azo phenyl monomer of formula (I). R=formula (i); and z, y=not defined. n=2-9. An INDEPENDENT CLAIM is included for a method of preparing the multi-environment responsiveness triblock copolymer comprising: (A) subjecting polyethylene glycol and methyl acrylic dimethylamine ethyl ester monomer to atom transfer radical polymerization in the presence of a solvent, catalyst and initiator at 20-60 degrees C for 1-12 hours, adding tetrahydrofuran, leaching, precipitating using n-hexane, filtering, and vacuum drying obtained filter cake to obtain polyethylene glycol polymethylacrylic acid dimethylamine ethyl ester di-block copolymer; and (B) adding solvent A and polyethylene glycol-b-polymethylacrylic acid dimethylamine ethyl ester di-block copolymer as initiator, introducing nitrogen to eliminate oxygen, adding catalyst system, heating at 20-60 degrees C for 6-24 hours, passing through neutral alumina column, eluting with tetrahydrofuran, concentrating the eluate, precipitating using diethyl ether, filtering, and vacuum drying.

参考文献:

正在载入数据...

版权所有©华东理工大学 重庆维普资讯有限公司 渝B2-20050021-7 
渝公网安备 50019002500408号 违法和不良信息举报中心