详细信息
Synthesis and characterisation of castor oil-urethane acrylate oligomers ( SCI-EXPANDED收录)
文献类型:期刊文献
英文题名:Synthesis and characterisation of castor oil-urethane acrylate oligomers
作者:Wang, Z; Gao, P
机构:[1]E China Univ Sci & Technol, Petrochem Inst, Shanghai 200540, Peoples R China;[2]Shanghai Jiao Tong Univ, Dept Chem, Shanghai 200240, Peoples R China
年份:2001
卷号:84
期号:1
起止页码:21
外文期刊名:SURFACE COATINGS INTERNATIONAL PART B-COATINGS TRANSACTIONS
收录:;WOS:【SCI-EXPANDED(收录号:WOS:000171805900003)】;
语种:英文
摘要:Castor oil-urethane acrylate (CVA) oligomers have been synthesised and characterised by intra-red spectroscopy (FT-IR), gel permeation chromatography(GPC) to study the relationship between the reaction kinetics and the structure of the products. It is shown that the chain terminating reaction between 2,4-toluene diisocyanate (2,4TDI) and hydroxyethylacrylate (HEA) to form isocyanatoethyl acrylate (IEA) obeys a second order mechanism, as does the chain extension reaction of IEA and castor oil (CAS). From the data of the polymerisation rate constant and the apparent activation energy, it can be seen that the different structure of CVA oligomer is dependent mainly on the different reactivities of both para and ortho NCO groups in 2,4TDI. Whereas the apparent viscosity of the CVA oligomer is related to the structure of diisocyanates. Results from the dynamic mechanical spectrum (DMS, the abstract of dynamic mechanical spectrum, a kind of detection method) indicate that the hard segment content of oligomers is then increased up to 59% (wt.). A phase-separated structure is formed and leads to the highest tensile strength (18.2MPa). When the hard segment content is increased to 67% (wt.), the dynamic modulus is reduced and the single depletion peak from DMS is exhibited at the temperature of 100.7 degrees.
参考文献:
正在载入数据...