详细信息
Preparing antistatic water solution comprises mixing water solution of poly(sodium p-styrenesulfonate), adding de-ionized water in the poly(3,4-ethylenedioxythiophene) solution, adjusting pH, and adding potassium persulfate
文献类型:专利
英文题名:Preparing antistatic water solution comprises mixing water solution of poly(sodium p-styrenesulfonate), adding de-ionized water in the poly(3,4-ethylenedioxythiophene) solution, adjusting pH, and adding potassium persulfate
作者:DONG R;GAO L;GOU W;LI B;MAO S;QIU C;WANG J;YANG J
机构:[1]UNIV EAST CHINA SCI & TECHNOLOGY
申请号:CN101434770-A
申请日:2008-11-28
公开日:2009-05-20
语种:英文
收录:DERWENT
摘要:NOVELTY - Preparing antistatic water solution comprises: (a) mixing water solution of poly(sodium p-styrenesulfonate) with solid content of 21.98 wt.% and 3,4-ethylenedioxythiophene at a weight ratio of 1:(1-5), stirring for 10-15 minutes, and obtaining poly(3,4- ethylenedioxythiophene) solution; and (b) adding de-ionized water in the poly(3,4-ethylenedioxythiophene) solution, making solid content be 1-1.5 wt.%, adjusting pH to 1-1.5, adding potassium persulfate, stirring magnetically for 24 hours, generating 3,4-ethylenedioxythiophene/poly(sodium p-styrenesulfonate) solution. USE - The method is useful for preparing antistatic water solution (claimed). ADVANTAGE - The invention is simple to operate and does not need advanced equipment. DETAILED DESCRIPTION - Preparing antistatic water solution comprises: (1) mixing water solution of poly(sodium p-styrenesulfonate) with solid content of 21.98 wt.% and 3,4-ethylenedioxythiophene at a weight ratio of 1:(1-5), stirring for 10-15 minutes, and obtaining poly(3,4- ethylenedioxythiophene) solution; and (b) adding de-ionized water in the poly(3,4-ethylenedioxythiophene) solution, making solid content be 1-1.5 wt.%, adjusting pH to 1-1.5, adding potassium persulfate, stirring magnetically for 24 hours, generating 3,4-ethylenedioxythiophene/poly(sodium p-styrenesulfonate) solution, where weight ratio of the 3,4-ethylenedioxythiophene to potassium persulfate is 1:(1-3), stirring speed is 800-1600 revolution/minute.
参考文献:
正在载入数据...