详细信息

Coke deactivation of Pd/H-mordenite catalysts used for C5/C6 hydroisomerization  ( SCI-EXPANDED收录)  

文献类型:期刊文献

英文题名:Coke deactivation of Pd/H-mordenite catalysts used for C5/C6 hydroisomerization

作者:Li, CL; Novaro, O; Mu?oz, E; Boldú, JL; Bokimi, X; Wang, JA; López, T; Gómez, R

机构:[1]Univ Nacl Autonoma Mexico, Inst Phys, Mexico City 01000, DF, Mexico;[2]E China Univ Sci & Technol, Petr Proc Res Ctr, Shanghai 200237, Peoples R China;[3]Inst Politecn Nacl, Super Sch Chem Engn, Lab Catalysis & Mat, ESIQIE,UPALM, Mexico City 07738, DF, Mexico;[4]Univ Autonoma Metropolitana IAP, Dept Chem, Mexico City 09340, DF, Mexico

年份:2000

卷号:199

期号:2

起止页码:211

外文期刊名:APPLIED CATALYSIS A-GENERAL

收录:;WOS:【SCI-EXPANDED(收录号:WOS:000087088500004)】;

语种:英文

外文关键词:coke composition; hydroisomerization; Pd/H-mordenite; catalyst; deactivation by coke; pilot plant

摘要:Coke formation in C-5/C-6 alkane isomerization on a Pd/H-Mordenite catalyst discharged from a pilot reactor was studied. Experimental techniques like XRD, EPR, MAS-NMR, FTIR, TGA and TPO, were applied for the characterization of coke and coked catalysts. It was shown that coke content, chemical composition, its structure and nature depended upon time-on-stream and section of the catalyst bed. The coke content increased from 3.0 in the top section, to 4.1 wt.% in the central section and 6.2 wt.% in the bottom of the catalyst bed and C/H ratio of the corresponding coke increased from 1:1.12, 1:0.55 to 1:0.35, which significantly affected the catalytic behavior and regeneration of the catalysts. The selectivity to 2,2-dimethyl butane during n-hexane isomerization, respectively, decreased from 19% for the fresh catalysts, to 10% and 8.3% for the coked catalysts in the central and outlet sections. As time-on-stream increased, coke initially formed on palladium metals and then moved to acidic sites in the support where polyaromatic or pseudographite-like structures were formed through further acid catalyzed reactions. Two kinds of coke with different nature could be combusted below 300 and 600 degrees C, respectively. These results are very useful for choosing operation parameters to restore initial activity of the coked catalysts in the regeneration units in our pilot plant. (C) 2000 Elsevier Science B.V. All rights reserved.

参考文献:

正在载入数据...

版权所有©华东理工大学 重庆维普资讯有限公司 渝B2-20050021-7 