详细信息

Microwave-accelerated direct regeneration of LiCoO_(2)cathodes for Li-ion batteries    

文献类型:期刊文献

中文题名:Microwave-accelerated direct regeneration of LiCoO_(2)cathodes for Li-ion batteries

作者:Xueshan Hu[1,2,3];Yun-Chao Yin[1];Chao Li[1];Lihui Zhou[4];Lin Yang[2];Yitian Feng[2];Daxian Zuo[2];Chenhui Ning[2];Das Soham[5];Sheng Dai[4];Longbin Qiu[2];Lin Zeng[2];Haw Jiunn Woo[3];Jiayu Wan[1]

机构:[1]Future Battery Research Center,Global Institute of Future Technology,Shanghai Jiao Tong University,Shanghai 200240,China;[2]Department of Mechanical and Energy Engineering,Southern University of Science and Technology,Shenzhen 518055,China;[3]Centre for Ionics University of Malaya,Department of Physics,Faculty of Science,University of Malaya,Kuala Lumpur 50603,Malaysia;[4]Key Laboratory for Advanced Materials and Feringa Nobel Prize Scientist Joint Research Center,School of Chemistry and Molecular Engineering,East China University of Science and Technology,Shanghai 200237,China;[5]Department of Natural and Applied Sciences,Duke Kunshan University,Kunshan 215316,China

年份:2024

卷号:67

期号:7

起止页码:2181

中文期刊名:Science China Chemistry

外文期刊名:中国科学(化学英文版)

收录:CSTPCD;;Scopus;CSCD:【CSCD2023_2024】;PubMed;

基金:supported by the startup funding of Shanghai Jiao Tong University;the National Natural Science Foundation of China;the Ministry of Higher Education of Malaysia for the Fundamental Research Grant(FRGS/1/2022/STG05/UM/02/3)to Woo Haw Jiunn。

语种:英文

中文关键词:battery recycling;spent lithium cobaltate;microwave;directly regeneration;cathode materials

摘要:Recycling spent lithium-ion batteries is integral to today's low-carbon environmental protection efforts.The concept of direct regeneration,acknowledged for its environmental sustainability,economic viability,and consistent performance of recycled materials,is gaining prominence.This study presents an efficient and nondestructive approach by utilizing an ultrafast microwave technology to directly regenerate spent lithium cobaltate(LCO)cathode materials.In contrast to conventional furnacebased processes,this method significantly reduces the regeneration timeframe.By subjecting the spent LCO mixed with lithium sources to three microwave heating cycles(at approximately 1,350 K),LCO regeneration is achieved,yielding a specific capacity of 140.8 mAh g^(-1)(0.2 C)with a robust cycle stability.With further environmental and economic benefits,the ultrafast microwave technology holds scientific promise for directly regenerating cathode materials,while establishing competitiveness for industrial applications.