中文题名:激光烧蚀法制备NiSO_4/Ni(Ac)_2纳米粒子
英文题名:Nanoparticles of NiSO_4/Ni(Ac)_2 Prepared with Laser Ablation
作者:金桂林[1];金晓英[1];陈建华[1];黄洪成[1]
机构:[1]华东理工大学物理系,上海200237
年份:2003
卷号:23
期号:2
起止页码:84
中文期刊名:应用激光
外文期刊名:Applied Laser
收录:CSTPCD;;北大核心:【北大核心2000】;CSCD:【CSCD2011_2012】;
语种:中文
中文关键词:激光烧蚀法;NiSO4;Ni(Ac)2;纳米粒子;硫酸镍
外文关键词:laser ablation nanoparticles NiSO 4 Ni(Ac) 2
摘要:硫酸镍与乙酸镍的混合晶体经研磨成 2 μm的颗粒后 ,压制成直径为 10mm的薄片作为靶材 ,以TEACO2 激光辐照 ,得到粒度为 10至 2 0nm的NiSO4/Ni(Ac) 2 纳米粒子 ,其中含少量Ni2 O3 。气体产物为水和乙酸。激光功率密度为 10 8W .cm-2 量级。讨论了激光作用的机理。
TEA CO 2 laser beam was used to irradiate the mixed crystal of NiSO 4 and Ni(Ac) 2 , which had been grained into powders of 2μm size and then pressed into pieces of 10 mm diameter as target material. Nanoparticles of NiSO 4/Ni(Ac) 2 , containing a little Ni 2O 3 , were prepared. The size of which was 10 to 20 nm. And the gas products were H 2O and CH 3COOH. The laser power density was of 10 8 W.cm - 2 order of magnitude. The mechanism of laser action is discussed. A method of laser ablation for preparing nanoparticles, the chemical composition of which is as similar to that of the target material as possible, is being offered.