详细信息

Normal Hexane Hydroisomerization Over Alumina Modified Pt/SO4 2-/ZrO2 Catalyst  ( SCI-EXPANDED收录 EI收录)  

文献类型:期刊文献

英文题名:Normal Hexane Hydroisomerization Over Alumina Modified Pt/SO4 2-/ZrO2 Catalyst

作者:Xiao, Y. P.[1];Wang, Z. Y.[2];Zhang, Y. F.[2];Song, Y. Q.[2];Zhou, X. L.[2];Li, C. L.[2]

机构:[1]China Petr Chem Corp, Anqing Petrochem Branch Corp, Anqing, Anhui, Peoples R China;[2]E China Univ Sci & Technol, Petr Proc Res Ctr, Shanghai 200237, Peoples R China

年份:2013

卷号:31

期号:3

起止页码:331

外文期刊名:PETROLEUM SCIENCE AND TECHNOLOGY

收录:;EI(收录号:20130415935899);WOS:【SCI-EXPANDED(收录号:WOS:000313942400012)】;

基金:The authors would like to thank the financial supports from the key international cooperative research projects by National Ministry of Science and Technology, P. R. China (No. 2004CB720603), and Postdoctoral Science Foundation of P. R. China (200902221).

语种:英文

外文关键词:alumina; hydroisomerization; n-hexane; platinum; sulfated zirconia

摘要:Pt/SO4 2-/ZrO2-Al2O3 (PSZA) catalysts were prepared by extruding sulfated hydroxide zirconium with SB powder. The n-hexane hydroisomerization reaction was performed in a continuous flow fixed-bed reactor. Isomerization activities under varying pretreatment parameters (including catalyst storage time before use, activating temperature, and reduction temperature) and reaction conditions (including reaction temperature, space velocity, and the molar ratio of hydrogen to n-hexane) were investigated. The results indicated the optimum pretreatment conditions for the PSZA catalyst is as follows: five days of storage, 350 degrees C of the activation temperature, and 250 degrees C of the reduction temperature. In addition, the optimum reaction conditions contained the reaction temperature ranging from 200 to 210 degrees C, space velocity of 1 hr-1, and hydrogen to hexane mole ratio of 5.