Research of mica/Fe3O4 pearlescent pigment by co-precipitation ( SCI-EXPANDED收录)
文献类型:期刊文献
英文题名:Research of mica/Fe3O4 pearlescent pigment by co-precipitation
作者:Liang Xiaojuan[1,3];Xu Haiquan[2];Chen Jing[2];Sun Juncai[1];Yang Yuxiang[2];Liu Xiangnong[4]
机构:[1]Dalian Maritime Univ, Dalian 116026, Peoples R China;[2]E China Univ Sci & Technol, Dept Chem, Shanghai 200237, Peoples R China;[3]Wenzhou Univ, Coll Chem & Mat Engn, Wenzhou 325035, Peoples R China;[4]Yangzhou Univ, Testing Ctr, Yangzhou 225009, Peoples R China
年份:2011
卷号:37
期号:3
起止页码:330
外文期刊名:GLASS PHYSICS AND CHEMISTRY
收录:;WOS:【SCI-EXPANDED(收录号:WOS:000292210600011)】;
基金:Project supported by the National Natural Science Foundation of China (no. 20971043) and Zhejiang Province Science Foundation (no. 2006C1118).
语种:英文
外文关键词:co-precipitation; pearlescent pigment; mica
摘要:Experiments on preparation of mica/Fe3O4 pearlescent pigment were performed to discuss influences of several crucial parameters on final products. The samples were characterized by XRD, HRSEM, FTIR and color measurement, the content of Fe3O4 on the mica surface was also analyzed by XPS. It was found that the smoothness, compactness and colour deepness of the coating were influenced by different pH values and temperatures. The optimum preparation parameters of mica/Fe3O4 pearlescent pigment were obtained: the value of pH a parts per thousand yen 9.2; the concentration of sodium hydroxide was 0.5 mol/l; the concentration ratio of Fe3+ to Fe2+ was 1.6 : 1; the velocity of magnetic stirring was 138 a parts per thousand currency sign v a parts per thousand currency sign 151 r/min; reaction temperature was 70-80A degrees C; calcination temperature was 350A degrees C and calcination time was 3 h.